Cellulosic Welding Electrode for Vertical-Down Pipeline Girth Welding

Cellulosic Welding Electrode for Vertical-Down Pipeline Girth Welding

Brand NameHangzhou MetalWire Technology
Model NumberE6010
MOQ1 set
PriceNegotiable
Delivery Time45-60 days
Payment TermsT/T, L/C

Product Description

1. Overview

The cellulosic welding electrode has a high-cellulose coating and is designed for DCEP welding. It is intended for vertical-down welding of pipeline girth seams in all positions and is also suitable for general carbon steel structures. It produces a forceful, deep-digging arc and is suitable for single-sided welding with a clean root bead on the back side.

1.1 Standards

Standard Classification
AWS A5.1 E6010
GB/T 5117 E4310
ISO 2560-B E 43 10 A

2. Coating and Operating Characteristics

  • Coating: high-cellulose; designed for DCEP (direct current electrode positive) welding.
  • Vertical-down welding of pipeline girth seams in all positions.
  • Forceful arc with strong digging action.
  • Single-sided welding with a clean root bead on the back side.
  • Good resistance to porosity and hot cracking.
  • Typical applications: girth butt welding of 430 MPa-grade carbon steel pipelines and general carbon steel structures.

3. Deposited Metal Chemical Composition (%)

Element C Mn Si S P Ni Cr Mo V
Guaranteed ≤ 0.20 ≤ 1.20 ≤ 1.00 ≤ 0.035 ≤ 0.040 ≤ 0.30 ≤ 0.20 ≤ 0.30 ≤ 0.08
Typical 0.09 0.42 0.15 0.020 0.025 0.030 0.035 0.005 0.004

4. Deposited Metal Mechanical Properties

Property Tensile strength (Rm) Yield strength (ReL) Elongation (A) Impact energy (KV2) at -30 °C
Guaranteed ≥ 430 MPa ≥ 330 MPa ≥ 20% ≥ 27 J
Typical 475 MPa 400 MPa 26% 80 J

X-ray inspection: Grade II (defect-free).

Diameter (mm) 2.5 3.2 4.0
Length (mm) 300 350 350
Current (A), DCEP 50–80 60–100 100–140

6. Welding Positions and Operating Notes

The electrode is designed for vertical-down welding of pipeline girth seams in all positions.

  • Use DCEP for the root pass.
  • Keep the arc short and avoid excessive weaving.
  • Clean the joint area before welding.
  • Clean slag between passes in multi-layer welding.

Welding position diagram for the cellulosic pipeline electrode

View More